[mems-talk] Re: Copper plating
imran ali
aimsali813 at yahoo.com
Mon Feb 5 23:21:46 EST 2007
Hey Shay,
what i suggest is to add less proportion of acid to solution.
hope this will help?
regards
imran ali
From: "Shay Kaplan" <shay at mizur.com>
To: "'General MEMS discussion'" <mems-talk at memsnet.org>
Date: Sun, 4 Feb 2007 08:49:30 +0200
Subject: RE: [mems-talk] Copper plating
The copper diffuses into the gold
-----Original Message-----
From: mems-talk-bounces at memsnet.org [mailto:mems-talk-bounces at memsnet.org]
On Behalf Of Nik Dee
Sent: Saturday, February 03, 2007 4:19 PM
To: mems-talk at memsnet.org
Subject: [mems-talk] Copper plating
Hi guys, I am currently using a Copper plating solution (Water, Copper
Sulphate, Sulphuric Acid, NaCl and CUbath copper brightener) on gold seed
layer. I try to keep the plating rate to 30mA / cm2. I have noticed
sometimes that the copper plated on the seed surface is not bright enough
and it gets a pink colour. Do you have any idea what the reason for that
might be?