[mems-talk] deposit alloy
B Frank
benfrankm at gmail.com
Tue Feb 6 01:34:22 EST 2007
Hi, All,
I have a problem to deposit alloy in thermal evaporator system.
The alloy is Al(2% Si). During deposition, the silicon was left at the
boat, because the melting point of Si is much higher than Al.
The alloy is wire, so alreay mixed before i receive it.
Is there anybody have such experience? Is it possible to evaporate
such alloy in thermal evaporator system? How about deposit Au(1% Sb)?
Your suggestion will be deeped appreciated.
Thanks.