[mems-talk] SU-8 and S1813
Brubaker Chad
C.Brubaker at EVGroup.com
Fri Jan 5 13:51:47 EST 2007
Oh yes. It would most likely strip it, since SU-8 developer is the same
solvent as the casting solvent for S1813 (PGMEA - propylene glycol
monomethyl ether acetate, or 1-methoxy-2-propanol acetate)
Best Regards,
Chad Brubaker
EV Group invent * innovate * implement
Technology - Tel: 480.727.9635, Fax: 480.727.9700 e-mail:
c.brubaker at EVGroup.com, www.EVGroup.com
-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of Homan, Tony J
Sent: Thursday, January 04, 2007 2:40 PM
To: mems-talk at memsnet.org
Subject: [mems-talk] SU-8 and S1813
Hi all-
Does anyone know if the SU-8 developer would damage a layer of S1813
deposited under SU-8?
More information about the MEMS-talk
mailing list