[mems-talk] How to clean PDMS or PLGA thin film on the Si chip
Barbara Cortese
KORTESEB at libero.it
Thu Jan 11 02:48:08 EST 2007
You can't clean pdms with solvents but you can try dry etching (RIE) with O2!
> Hi, I have tried several ways to clean the PDMS thin film on the Silicon
> pattern(including HF, Piranha,etc). But the result is not good and
> especially I want to clean the PDMS in the hole of Si chip. Does anybody
> know how to clean it or any paper mentioned the way of cleaning?