[mems-talk] wet etch recipe for Iridium (Ir)

Mantavya <Manu> Sinha mantavya at gmail.com
Sat Jan 27 22:35:54 EST 2007


hi guyz,
can anyone tell me the wet etch recipe for Iridium (Ir). It seems to be
quite resistive to hot(85'C) dilute(1:1) aqua regia. Also it should have
selectivity over IrSi.
Looking forward to hearing from you people.

Warm Regards,
Manu