Hello members,
I was wondering if I could find a resin which could resist to DMF.
Actually, I have to fabricate several pools into PMMA and I'd like to
depose a drop of DMF .
Unlikely PMMA doesn't resist to DMF.
Could you tell me if I can find a resin able to resist to DMF?
Thank you very much.
--
*********************************************************