[mems-talk] Platinum deposition problem

Jian Wang jian at flexcellint.com
Tue Jul 3 15:02:06 EDT 2007


Hi All,
   
  I made a SU8 2075 molds with Mylars mask. My problem is that all diagonal features are peeled off after 5-6 minutes in SU8 developer, while almost of all vertical and horizontal lines or dots are still firmly attached on the silicon wafer. Here are main steps of the protocol: clean Si wafer with BOE, spin coat SU8, soft bake, UV exposure, PEB and then SU8 developer. The diagonal features are 10 um (width) x 80 um (height), the other features are 40 um or up. By the way, this is my first time to use mylars mask for making SU8 2075 molds. I had no problem of using the similar protocol with glass/Cr masks for making other SU8 molds.
  Could somebody assist me with his/her own experience or suggest a reference?
   
  Wang