[mems-talk] AZ 5214 PR for metal lift off

jpt sharma jptsharma at yahoo.com
Mon Jul 23 14:45:21 EDT 2007


Hi all
  I am using AZ 5214 photoresist for metal liftoff. Do you have any idea about the solvent can be used for lift off other than Acetone? 
  Thanks in Advance.
   
  John