[mems-talk] Depositing metals onto plastics and SU-8
Mantavya Sinha
mantavya at nus.edu.sg
Fri Mar 2 22:50:04 EST 2007
You are right Roger. E-Beam is not going to be a cool process. In my
experience Sputtering should give you near room temperature (RT +
10'C-15'C) deposition.
Cheers
Mantavya Sinha
PhD Student
Dept of ECE
NUS
-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of Roger Shile
Sent: 03 March 2007 09:41 AM
To: 'General MEMS discussion'
Subject: RE: [mems-talk] Depositing metals onto plastics and SU-8
Contrary to many postings here, E-beam evaporation is thermal
evaporation; the charge is not cool by any means.
Roger Shile
More information about the MEMS-talk
mailing list