[mems-talk] E-beam evaporation with Silver

Shay Kaplan shay at mizur.com
Wed Mar 14 09:25:40 EST 2007


Hi
Silver evaporates just fine. No problems. If you're going to evap only few
times you might want to line the surfaces with aluminum foil just as with
any other material. 
Shay

-----Original Message-----
From: mems-talk-bounces at memsnet.org [mailto:mems-talk-bounces at memsnet.org]
On Behalf Of Siripon Sukuabol
Sent: Wednesday, March 14, 2007 7:42 AM
To: mems-talk at memsnet.org
Subject: [mems-talk] E-beam evaporation with Silver

HI..All,

Please advise... Anybody has ever deposited Silver (99.99%) on the silicon
wafer by using E-beam evaporation machine....

Does Silver have any effects with E-beam Chamber and machine? 
For example, it makes chamber dirty and hard to clean.