Hi Ciro,

our EVG 620 has a Nanoimprint module with a "contact free wedge error 
compensating". This means, that small flaps are automaticly put between 
the wafer and the mask, and you have no contact before they are aligned. 
I think that is what you want.

Bets regards,

Oliver Horn