[mems-talk] Bonding gold wires to gold electrode
shay kaplan
shay at mizur.com
Fri May 11 10:44:20 EDT 2007
Jeff
You might have a problem because the SU8 will absorb the US energy. For pad
on
Si or glass, 1500A of evaped or sputtered gold is enough - on SU8 I think
you will need a thicker layer.
Shay
-----Original Message-----
From: Yue Mun Pun, Jeffrey
Sent: Friday, May 11, 2007 4:30 PM
To: mems-talk at memsnet.org
Subject: [mems-talk] Bonding gold wires to gold electrode
Hi,
I need to bond gold wires to gold electrode. Typically, how thick should
the gold electrode be and what should the surface area of the electrode be
for a good bond?
Also, will there be any impact if the gold electrode is sitting on a film of
SU-8, for if ultrasound is used in the bonding process, I'm afraid that the
underlying SU-8 might crack due to the high energy of the ultrasound.
More information about the MEMS-talk
mailing list