[mems-talk] How to etch SU8 from Nickel structure?

Dubnisheva, Anna dubnisha at ccf.org
Mon May 14 13:21:41 EDT 2007


Hi,

In my experience I never could remove SU-8 from the wafers after it was UV exposed and cross-linked. 
You may have to try Omni coat - look it up on Microchem website - and with it you will be able to remove SU-8.

Sincerely,
Anna

-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org]On Behalf Of Simon Zhang/gcemarket
Sent: Monday, May 14, 2007 12:06 PM
To: mems-talk at memsnet.org
Subject: [mems-talk] How to etch SU8 from Nickel structure?


Anyone knows good wet or dry etching method for etching SU8 from Nickel 
structure ?

Thanks and regards,

Simon Zhang
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe: 
http://mail.mems-exchange.org/mailman/listinfo/mems-talk


===================================




Cleveland Clinic is ranked one of the top 3 hospitals in
America by U.S.News & World Report. Visit us online at
http://www.clevelandclinic.org for a complete listing of
our services, staff and locations.


Confidentiality Note:  This message is intended for use
only by the individual or entity to which it is addressed
and may contain information that is privileged,
confidential, and exempt from disclosure under applicable
law.  If the reader of this message is not the intended
recipient or the employee or agent responsible for
delivering the message to the intended recipient, you are
hereby notified that any dissemination, distribution or
copying of this communication is strictly prohibited.  If
you have received this communication in error,  please
contact the sender immediately and destroy the material in
its entirety, whether electronic or hard copy.  Thank you.





More information about the MEMS-talk mailing list