[mems-talk] Activation of 'old' nickel surface

James Zhu james.zhu at epigem.co.uk
Wed May 23 11:31:26 EDT 2007


Hello, all. I want to give gold finish (electroless gold) on top of a
passivated nickel surface. I tried pre-dip in a 5% HCl solution before
gold plating, but the gold still can be peel off easily. Can anyone help
me to improve the gold adhesion to nickel. Thanks J. Zhu from Epigem,UK.



More information about the MEMS-talk mailing list