Hello everyone,

We work with Carbon nanotubes grown on copper foils using a nickel 
catalyst.  Once the tubes are formed, is there a process to deactivate 
or get rid of the nickel caps from the nanotubes without causing any 
structural damage to the surface?  Any help would be greatly 
appreciated.  Thanks!

-- 