Hello,

After undergoing a 1um wet oxidation @ 1050C, I notice a haze pattern on my silicon wafers. Sometimes there is ring of haze around the wafer edge while the center is clear. Other times, the center has haze while the edges are clear.

It is only visible under a strong white light.

Has anyone seen this occur on their wafers? Or come across literature that discuss this?