Use the SU-8 3000 series, you'll get much better results. SU-8 doesn't adhere that well to untreated glass.
-----Original Message-----
From: mems-talk-bounces at memsnet.org on behalf of Yue Mun Pun, Jeffrey
Sent: Wed 10/3/2007 4:58 AM
To: General MEMS discussion
Subject: [mems-talk] Adhesion of SU-8 and gold to glass wafer
Hi,
Can anyone tell me how I can ensure SU-8 and gold conductors adhere well to glass wafer? Thanks.