I may miss some comments. You can use SU-8 3000 for coating glass with better adhesion result. If you have to use SU-8 2000 products, try clean substrate surface with oxygen plasma or Piranha solution, dry it with a hot plate and increase the exposure time.
   
  Jian Wang
  Senior Scientist
  Flexcell International

"Yue Mun Pun, Jeffrey" <g0500396 at nus.edu.sg> wrote:
  Hi,
I am using SU-8 2000 series and may need to use it on glass wafers. Can anyone suggest how I can make SU-8 adhere to glass, whether I need to spin coat Omnicoat or treat the glass with oxygen plasma?