[mems-talk] Al2O3
Gary Hillman
garyh at s-cubed.com
Wed Oct 10 13:01:48 EDT 2007
J. Alumina is really pretty chemically resistant. The only thing that I
think will touch it is HF and then VERY slowly. Gary
-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org]On Behalf Of jpt sharma
Sent: Wednesday, October 10, 2007 11:57 AM
To: mems-talk at memsnet.org
Subject: [mems-talk] Al2O3
I am looking for the AL2O3 wet etch chemical. Can anyone suggest me the
chemical and vendor?