Dear Yang,

Many factors determine the final temperature. For examples, the substrate area 
materials' heat conductivity, and their heat capacity. Generally speaking, with 
the same heating power, smaller heating area can acheive higher local 
temperature. 

Best,

Joseph   

-- 
ChungHao Chen (Joseph)
Research Assistant
Purdue University
School of Electrical and Computer Engineering
EE Building Box 114
465 Northwestern Avenue
West Lafayette, IN 47907-2035
email: chen170 at purdue.edu



Quoting Steven Yang <steven030505 at gmail.com>:

> Hi,all
> To fabricate a micro heater with metal pattern, which metal is better,
> Al, Pt, or Au? Better means using low power to achieve the same
> temperature, lets say cost less than 10mW to get temperature around
> 100-200 degree with line width around 20um.
> 