[mems-talk] etching off plated nickel

Johnson Wong johnson.wong at unsw.edu.au
Mon Oct 29 21:55:56 EST 2007


Hi:

I recently tried to use nickel plating solution from transcene to
plate poly-Si.  Afterwards I tried etching the nickel off with piranha
etch but it left a hazzy film on the poly-Si, which I suspect is
nickel oxide.  Is there any way to etch off the nickel oxide without
etching the poly-Si?

Thanks and regards,
Johnson Wong
PhD Research
School of Photovoltaic Engineering
University of New South Wales
NSW 2052, Australia
Office (04) 9385 7942


More information about the MEMS-talk mailing list