[mems-talk] Nb wet etching
Kirt Williams
kirt_williams at sbcglobal.net
Sun Sep 23 20:13:53 EDT 2007
Do a Google search for "niobium etch rate mems."
The first paper you'll see has formulation and etch rates for Nb and a bunch
of other metals.
--Kirt Williams
----- Original Message -----
From: "Sadhana Patil" <ek.sadhana at gmail.com>
To: <mems-talk at memsnet.org>
Sent: Friday, September 21, 2007 6:48 PM
Subject: [mems-talk] Nb wet etching
> Hi all,
> Looking for some help on the kind of wet etchants available for etching
> Nb.
> I have vaguely heard about HF(1):HNO3(1). Does anybody have an idea of
> what is the etch rate of this chemical for Nb? Are there any other
> etchants available for Nb? And does it etch other metals like Au, Fe,
> CuMn, Ni?
> Thanks,
> ES...
More information about the MEMS-talk