Hi

I am looking for a process to remove Polyimide residues but not TiO2.  I 
can remove most of the polyimide with a Microstrip 2001 solution but 
there a still residues left. We know that a piranha clean would remove 
these residues but we are uncertain if it also attacks the titanium dioxide
Does anyone have an idea how we can remove the polyimide without 
damaging the (13-nm) TiO2 layer?
We also want to avoid the use of an O2-Plasma because that would damage 
our transistors.