Hi All,
Does anyone know of any chemical supplier/vendor selling ready-made phase-change plating solution? e.g. GeTe, Sb2Te3, Ge2Sb2Te5, etc.
I could not find any in the internet, so I currently mix the elemental powder with some acids and then used the mixture solution for phase-change material electrodeposition. But it's a tedious work, so It'll help much if there's any commercially available phase-change material plating solution.