[mems-talk] Hydrophobic treatments/coatings for Polycarbonate

Paul Monaghan p.monaghan at elec.gla.ac.uk
Thu Apr 10 03:57:18 EDT 2008


Hi Boris,

Thanks for the information. This sounds interesting, as does using Teflon AF 
described by Kevin Tsao. 112-115deg is right in in ball park of contact angles 
I am after.

Is your method proprietary? If not, can it be adapted using standard (and 
simple if possible!) lab methods? Is it possible you could forward some further 
details or alternatively point me in the right direction? 

Many thanks and best regards,

Paul

Quoting Boris Kobrin <boris_kobrin at appliedmst.com>:

> Hi Paul,
> 
> You can use simple vapor deposition method to change wettability of your
> polycarbonate. We usually getting 112-115 deg DI water contact angle on
> polycarbonate samples (depends on initial surface roughness). In-situ (vapor
> deposited) adhesion layer should be used in order to attach self-assembled
> hydrophobic monolayer to polymer materials, though total thickness of the
> dual layer can be kept below 100 A and the entire process is automated.
> 