[mems-talk] su8 1000um thick
Jian Wang
jian at flexcellint.com
Mon Apr 14 16:29:31 EDT 2008
Dr. Amit Asthana of Chungnam National University supplied an unpublished
protocol in this forum around last September. The method worked for making 1
mm thick SU8. You can search the list.
Jian Wang
Senior Staff Scientist
-----Original Message-----
From: mems-talk-bounces at memsnet.org [mailto:mems-talk-bounces at memsnet.org]
On Behalf Of Abhishek Jain
Sent: Sunday, April 13, 2008 12:28 PM
To: General MEMS discussion
Subject: [mems-talk] su8 1000um thick
Dear forum members
I want to make 1mm thick structures on SU8 for doing soft lithography with
PDMS later on. It is only one mask and just straight channels.
I have SU8 2075 with me and I am trying to find a recipe for doing this. If
anyone has experience in dealing with this, I will truly appreciate if you
may give some insight on the method...
More information about the MEMS-talk