I had a whole directory full or epapers. I'll try to find it and email some
to you.
Cheers
Shay
-----Original Message-----
From: mems-talk-bounces at memsnet.org [mailto:mems-talk-bounces at memsnet.org]
On Behalf Of Andrea Mazzolari
Sent: Sunday, April 20, 2008 3:42 PM
To: shay kaplan
Cc: mems-talk at memsnet.org
Subject: Re: [mems-talk] Silicon fracture strength
Hello Shay,
for my application at least one sufaces must be polished, the other one can
be etched. I can realize such crystals with pure chemical wet etching
methods, so crystal quality in the edge will be perfect.
Do you have any reference for the cited values ?
Many thanks,
Andrea