[mems-talk] Ni plating on Au film

Petru Lunca Popa petrulp at gmail.com
Wed Aug 6 10:22:11 EDT 2008


Hi
I am also plating Ni on Au using a Ni sulfamate solution
CAn you please tell me more detrails about you Ni plating proicess?
What solution you use?  What plating potentials?

On Sun, Jul 20, 2008 at 11:07 AM, Moshe <moduli0621 at yahoo.com> wrote:
> Nickel strike is a thin  intermediate film that made from 210 gr/ liter Nickel Chloride , 90ml/liter HCl - and the rest is DI water .
> This  intermediate make the adhesion bettwen the metal and the Nickel.
> It usually use to make adhesion between stainless steel and Nickel.