[mems-talk] Screen printing vendors for depositing epoxy glue

Adamson, Steve sadamson at asymtek.com
Wed Aug 13 11:53:26 EDT 2008


Almost any screen printer can do this. Your problem will be with
material choice. How long the pot life of the epoxy is. Is the glue
thixotropic and how well will it print. The you have to think about how
much glue you will waste on the screen and clean up. 

If you just want to make a few parts screen printing is a reasonable
method of deposition, however there are lots of dispensing tools on the
market, from simple hand held low cost systems to full in line high
performance systems. It depends on your application as to the type of
system to choose. 

Regards,
 
Steven J. Adamson
President IMAPS
 
Market Manager, Asymtek
 
 
-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of Xixixi Hahaha
Sent: Tuesday, August 12, 2008 3:53 PM
To: mems-talk at memsnet.org
Subject: [mems-talk] Screen printing vendors for depositing epoxy glue

Hello,
     I'm looking for a vendor which can prodive for dispensing or
depositing
epoxy glue using a screen-printing technique. Any information will be
appreciated.

Best Regards,

Vivian