[mems-talk] Lift-off method for ALD deposited Al2O3 with PMMA pattern
Jun Huang
huangking1 at gmail.com
Fri Aug 29 13:35:53 EDT 2008
Thanks. Actually I have already tried the method used in the APL paper
(scratch the surface, sonication,etc). But it just doesn't work. Maybe I
will try to use NanoStrip to remove PMMA layer.
Best regards,
Jun
On Fri, Aug 29, 2008 at 1:01 PM, Roger Shile <rshile at nanoink.net> wrote:
> Atomic Layer Deposition is conformal deposition process. I would,
> therefore, have expected some difficulty doing liftoff.
> However Google search for "ald liftoff" returned the following which you
> might find helpful,
>
> Low-temperature atomic-layer-deposition lift-off method for
> microelectronic
> and nanoelectronic applications
> APPLIED PHYSICS LETTERS VOLUME 83, NUMBER 12 22 SEPTEMBER 2003, p.2405
>
> Roger Shile
More information about the MEMS-talk
mailing list