[mems-talk] Si/Ge pieces surface cleaning

Xiaochen Sun sunxc at MIT.EDU
Tue Feb 5 15:13:30 EST 2008


Hi Ed,

Thank you very much for your advice. IPA is isopropyl alcohol right? I don't
think we have IPA dryer machine available now. I'll try rinse water off with
IPA and then blow dry with N2 first and see. 