You can buy wafer dicing saw blades and put them onto milling machines.
Its not elegant but it does work.
Regards,
Steven J. Adamson
President IMAPS
Market Manager, Asymtek
-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of
R.Loiacono at surrey.ac.uk
Sent: Wednesday, February 06, 2008 8:50 AM
To: Haixin.Zhu at asu.edu; mems-talk at memsnet.org
Subject: RE: [mems-talk] Dicing saw
Following this post, I have the same problem. I have been looking on the
internet for a long time, but basically dicing saws (for silicon, in my
case) are really bulky, big and expensive. It would be nice to have a
dicing saw that can just be put on a table for cutting wafers or dicing
smaller samples.
Any suggestions?