wouldn't just oxide work for you? if the phosphoric acid is pre-conditioned,
oxide is an excellent etch stopper.

_iv

On Jan 8, 2008 7:48 AM, Sandip Agarwal <sagarwal at nanoterra.com> wrote:

> I want to pattern silicon nitride by etching with hot phosphoric acid.
> What are the photoresists that would withstand these etching conditions?