Hi, All,
I didn't put the condition right in the previous email. The starting
wafer is heavily doped. Here is the question again:
I'm considering grow a silicon oxide layer on a heavily doped silicon
wafer through wet or dry oxidation
process. The question is: will the oxide layer obtained in such a way be
conductive? Advices are appreciated.
Best regards
Wenlin Jin
-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of Wenlin Jin
Sent: Tuesday, January 08, 2008 5:10 PM
To: General MEMS discussion
Subject: [mems-talk] conductivity of SiO2 layer grown on top of
heavilydoped silicon
Hi, All,
I'm considering grow a silicon oxide layer on a heavily doped silicon
wafer through wet or dry oxidation
process. The question is: will the oxide layer obtained in such a way be
conductive? Advices are appreciated.
Best regards
Wenlin Jin
More information about the MEMS-talk
mailing list