[mems-talk] diffusion constants in GaAs
Mantavya Sinha
mantavya at nus.edu.sg
Tue Jan 29 21:57:07 EST 2008
For gold, just look it up in Physics of Semiconductor Devices by S. M. Sze.
Manu
-----Original Message-----
From: mems-talk-bounces at memsnet.org [mailto:mems-talk-bounces at memsnet.org] On Behalf Of Bahram Ganjipour
Sent: Wednesday, January 30, 2008 3:12 AM
To: mems-talk at memsnet.org
Subject: [mems-talk] diffusion constants in GaAs
Hello Everyone,
I am looking for the diffusion constants of gold in GaAs , Platinum in GaAs and Nickel in GaAs. I would greatly appreciate any guidance
towards papers or reference volumes that might include this information.
I have come up dry with a number of different references, including the
CRC Handbooks.
Thank you very much for your help
More information about the MEMS-talk
mailing list