[mems-talk] adhesion problem for SU-8 on Si when hot-embossing

Meifang Lai meifang at mech.uwa.edu.au
Wed Jul 9 05:50:37 EDT 2008


Hi all,

I am developing a mold for hot-embossing by using SU-8 2050 on Si wafer. At present, I can get beautiful structures on Si after the photolithography process  (including hard bake at 150 ⁰C for 30 min). However, when I was trying to transfer the structure to PMMA (1 inch square) by hot embossing (pressure is 300 Kg, 125 ⁰C for 10min, and the demolding temperature is 90 ⁰C), all the Su-8 structures stayed in PMMA and separated from Si wafer. I have tried the HMDS, but it seems no difference. Does anyone have similar experience? Any suggestion will be appreciated.

Cheers,

Meifang


More information about the MEMS-talk mailing list