Hello,

I am looking to deposit an insulating, optically clear, layer for some
circuitry, and was wondering if I could Ebeam evaporate Silicon nitride?
Also, if I can, I saw something about alpha and beta forms, is there any
substantial difference when dealing with the insulating properties?