Sorry but what is Ni strike?
2008/7/17, Qi Luo <luoqi_101 at yahoo.com>:
> In our structure, we electroplate Ni on Au substrate. Our process has
> Alkaline clean, another step of activation, Ni strike, then Ni plating. For
> our application, the adhesion of the plated Ni to Au film is very important.
> Can we replace the Ni strike with Au strike, or insert a Au strike before Ni
> strike to improve adhesion? Your help would be greatly appreciated.
> With kind regards,
> Qi Luo