[mems-talk] Black wax

bob hou managerbcm02 at yahoo.com
Tue Jul 22 01:04:43 EDT 2008


this wax protective layer only can work for 1hour at 60 degree, i think.

--- On Mon, 7/7/08, 汪飞 <wangfeiustc at gmail.com> wrote:

From: 汪飞 <wangfeiustc at gmail.com>
Subject: Re: [mems-talk] Black wax
To: "General MEMS discussion" <mems-talk at memsnet.org>
Date: Monday, July 7, 2008, 11:50 PM

What do you mean about "that this protective film only takes about an
hours in KOH 40% at 60ºC"?

2008/7/4, Anahí Weinstock <wanahi at inti.gov.ar>:
> Hi
> I´m using black wax as wet etching protector. In bibliografy it is
> dissolved in toluene and cured at 100 ºC in oven for 1 hs, then after
> being deposited on the wafer. The problem is that this protective film
> only takes about an hours in KOH 40% at 60ºC.
> Someone has experience what are the optimal conditions for working with
> this material?
> Thanks
> Anahí

-- 
Best regards,
Yours sincerely
Fei Wang
______________
State Key Lab of Transducer Technology,
Shanghai Institute of Microsystem and Information Technology,
Chinese Academy of Sciences
865 Changning Road, Shanghai 200050, China
Email:wangfeiustc at gmail.com
Tel:0086-21-62511070 ext.5468


More information about the MEMS-talk mailing list