[mems-talk] Photoresist to withstand acidic anodization

pradeep # sharma psharma_02 at rediffmail.com
Sun Jun 1 00:54:57 EDT 2008


Dear Friends,

We intend to do anodization of aluminum foil in sulphiric acid, oxalic acid and phosphoric acid. Anodization voltage will be 25 V to 100 V and concentrations of acids will be about 4 percent by weight. 

We need to put a photoresist on Al surface and then open 2 micron diameter circles in photoresist by photolithography. 

Please suggest some resist for our purpose. Make sure the resist can withstand the acids, and have adequate breakdown voltage and offers resolution of about 0.5 to 1 micron.. 
  
Thanks to all. 

with love and best wishes,
Pradeep Sharma, 

Laboratory NB 02, 
IAMS, Academia Sinica, 
P.O. Box: 23-166,
Taipei-106, Taiwan, R.O.C.

Phone Number: 00886-2-2362-4901 (Laboratory)
              00886-910984500 (Mobile)  




More information about the MEMS-talk mailing list