[mems-talk] 20um features using AZP4620

Haixin Zhu Haixin.Zhu at asu.edu
Tue Jun 3 16:26:17 EDT 2008


Dear all,

I am trying to produce 20um features using AZP4620, the thickness is
required to be 38um, I tried double coating/triple coating with various
spin speed and baking condition, and they did not work. Is there any one
having this experience and advise me on the right direction?