[mems-talk] Adhesion b/w Ni and electroplated Cu
Sardar Bilal
sardar.bilal at gmail.com
Fri Jun 13 10:27:21 EDT 2008
Hi,
I am working on deposition of Ni on electroplated Cu. The Ni, I have
deposited, has very poor adhesion to electroplated Cu and peels off during
the Cu seed layer etch in Perchloric Acid [HClO4]and Ce (NH4)2(NO3)6
solution. The Ni is deposited by evaporation. I would like to know:
1. What cleaning and drying step I should perform before evaporation to
improve adhesion ?I only remove the copper oxide in 10% nitric acid before
Ni deposition.
2. The effect of chamber pressure and rate of evaporation on Ni adhesion ?
and 3. Will an intermediate layer of Cr ( ca. 5 - 10 nm) help ?
I hope someone can help me on this !
cheers !
Bilal
TKK, Finland
More information about the MEMS-talk
mailing list