Tell me more about the critical dry procedure.  I manufacture vacuum
driers and anti stiction coating equipment.  I may have a suggestion.

Bill Moffat 

-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of Ramakrishna Kotha
Sent: Thursday, June 26, 2008 12:34 AM
To: mems-talk at memsnet.org
Subject: [mems-talk] Critical Dry

Hi,
 
I am performing critical dry to release a parallel plate structure,
which has SiO2 as a sacrificial layer

After removing the sacrifical layer-SiO2 with BOE, then the device is
transffered to DI Water and then to Acetone in the critical dry chamber.
After performig critical dry process using Polaron-CPD 7501 tool, all
the structures are damaged (due to stiction problem). 

Can anyone, suggest me the accurate process to perform critical dry.
 
 
Thanks in advance
Rama
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk


More information about the MEMS-talk mailing list