[mems-talk] keeping PDMS level
Bill Moffat
BMoffat at yieldengineering.com
Thu Jun 26 17:29:18 EDT 2008
How about vacuum baking to extract solvent rapidly. Bill Moffat
-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of Sarosh Khwaja
Sent: Thursday, June 26, 2008 2:10 PM
To: jose.dr.g at gmail.com; General MEMS discussion
Subject: Re: [mems-talk] keeping PDMS level
Just an idea, how about spinning it at a very low RPM?
On Wed, Jun 25, 2008 at 5:32 PM, Jose Guevarra <jose.dr.g at gmail.com>
wrote:
> Hi,
>
> i'm working with PDMS. when I cure the PDMS and let it stand for
> about 24 hours I need to keep it level. Eve-balling how level it is
> doesn't seem to work very well. Does anyone know of a simple way of
> keeping PDMS level as it solidifies?
>