Hi,
I am not sure which pdms you are using, photopatternable or normal
Sylgard thing. If you are using sylgard 184 then keep it in oven for 45 mins
at around 110deg cent.
Secondly if your structures are very large they will be concave upto
certainextent as pdms solidifies faster at corners and edges bec of more
surface area frm where solvent evaporates.
Best luck
Yusuf
On Thu, Jun 26, 2008 at 11:10 PM, Sarosh Khwaja <sarosh.lists at gmail.com>
wrote:
> Just an idea, how about spinning it at a very low RPM?
>
> On Wed, Jun 25, 2008 at 5:32 PM, Jose Guevarra <jose.dr.g at gmail.com>
> wrote:
>
> > Hi,
> >
> > i'm working with PDMS. when I cure the PDMS and let it stand for about
> 24
> > hours I need to keep it level. Eve-balling how level it is doesn't seem
> to
> > work very well. Does anyone know of a simple way of keeping PDMS level
> as
> > it solidifies?
--
Mohd.Yusuf.S.Mulla