[mems-talk] pdms removal
Mohd.Yusuf
ysminstru at gmail.com
Sat Jun 28 12:27:18 EDT 2008
u can use Acetone to clean the dish. i am not sure about wafer...
yusuf
On Sat, Jun 28, 2008 at 4:50 PM, Jose Guevarra <jose.dr.g at gmail.com> wrote:
> Hi,
>
> I use a silicon wafer with su-8 as a mold in a petri dishfor PDMS. After
> the PDMS is solidified I remove it by peeling it off.
>
> How do I thoroughly clean off the solidified PDMS from the wafer and petri
> dish?
>
--
Mohd.Yusuf.S.Mulla
Student-FH Jena, Germany.
Currently at :- Leuven, Belgium
More information about the MEMS-talk