Sat Jun 28 18:42:23 EDT 2008
Hi,
Regarding this you can find very useful info in following paper. *
Characterization of Polydimethylsiloxane (PDMS) Properties
for Biomedical Micro/Nanosystems
*by *
Alvaro Mata,1,2 Aaron J. Fleischman,2
and Shuvo Roy2,∗
**
Biomedical Microdevices 7:4, 281–293, 2005
In this paper they have investigated almost all useful properties of PDMS in
different ratios etc.
Regards,
Yusuf
*
On Sat, Jun 28, 2008 at 6:04 PM, Jose Guevarra <jose.dr.g at gmail.com> wrote:
> Hi,
>
> I use the 10 to 1 base to curing agent ration for PDMS. I would like to
> make the PDMS more rigid. Would adding more curing agent make it more
> rigid?
>
> Thanks.
--