even this paper can help:

Carrillo F, Gupta S, Balooch M, Marshall S J, Marshall G W, Pruitt L and Puttlitz C M "Nanoindentation of polydimethylsiloxane elastomers: effect of crosslinking, work of adhesion, and fluid environment on elastic modulus"
J. Mater. Res. 20.10: 2820-2830 (2005)

A 3:1 or 5:1 should do for you.
Otherwise try h-pdms.

---------- Initial Header -----------

>From      : mems-talk-bounces at memsnet.org
To          : "General MEMS discussion" mems-talk at memsnet.org
Cc          : 
Date      : Sat, 28 Jun 2008 12:04:59 -0400
Subject : [mems-talk] pdms base/curing agent ration

> Hi,
> 
>   I use the 10 to 1 base to curing agent ration for PDMS. I would like 
> to make the PDMS more rigid.  Would adding more curing agent make it 
> more rigid?