[mems-talk] RE: MEMS-talk: Re: removing sticky adhesive (Olgierd
Cybulski)
Alderete, Michael
Michael.Alderete at drs-sts.com
Thu Mar 20 16:19:53 EST 2008
Olgierd-
Perhaps wafer dicing tapes leave fewer residues? Try some of the dicing
tape suppliers and see what they say.
Michael Alderete
Mechanical Packaging Engineer
DRS Sensors & Targeting Systems, Inc.
10600 Valley View St.
Cypress CA 90630-4833
michael.alderete at drs-sts.com
TEL (714) 220-4410
FAX (714) 220-5583
-----Original Message-----
Date: Wed, 19 Mar 2008 18:57:01 +0100
From: "Olgierd Cybulski" <olgierd.cybulski at gmail.com>
Subject: Re: [mems-talk] removing sticky adhesive
To: vikrant.c at iitb.ac.in, "General MEMS discussion"
<mems-talk at memsnet.org>
Message-ID:
<83cd18950803191057y31bd87f2p67ae79b4bcb20301 at mail.gmail.com>
Content-Type: text/plain; charset=ISO-8859-1
> is there a way to remove sticky adhesive, which is left over after a
> cellotape is removed. we are using cello tape for masking while
etching
> SiN, and when cellotape is peeled of the sticky glue is left over. Is
there
> a better way to remove it with out scrubbing?
It depends on the type of glue. Try IPA, extraction naphtha or benzine.
Sometimes acetone is enough.
More information about the MEMS-talk
mailing list