Vikrant,
Something you might try instead of standard cellophane tape is plater's
tape. It is made of kapton and has a low tack adhesive that works for
masking during plating operations, and also for some etches if they are not
too aggressive.
Brad Cantos
On 3/18/08 7:03 AM, "Vikrant A. Chaudhari :)" <vikrant.c at iitb.ac.in> wrote:
> hello,
>
> is there a way to remove sticky adhesive, which is left over after a
> cellotape is removed. we are using cello tape for masking while etching
> SiN, and when cellotape is peeled of the sticky glue is left over. Is
> there a better way to remove it with out scrubbing?